Inconel 660 / Alloy 660 (UNS S66286 / SUH660 / GH2132) – Superalloy Yochokera ku Iron Youma ndi Kuuma Yogwiritsidwa Ntchito Pakutentha Kwambiri

Kufotokozera Kwachidule:

Inconel 660 (UNS S66286 / SUH660 / GH2132 /W.Nr. 1.4980) ndi superalloy yolimba yochokera ku chitsulo yokhala ndi mphamvu yotentha kwambiri komanso yolimbana ndi okosijeni mpaka 704°C (1300°F). Womic Steel imapereka Inconel 660 m'njira zosiyanasiyana kuphatikizapo chitoliro chosasunthika, chitoliro cholumikizidwa, bala lachitsulo, mbale yachitsulo, coil yachitsulo, strip, flanges, fittings, forgings, waya, ndi zomangira za ndege, turbine ya gasi, magalimoto, nyukiliya, ndi petrochemical.


Tsatanetsatane wa Zamalonda

Ma tag a Zamalonda

Kodi Inconel 660 ndi chiyani?

Inconel 660 ndi nickel-chromium superalloy yopangidwa ndi chitsulo yomwe imalimbikitsidwa ndi kutsika kwa gawo la γ' [Ni₃(Al,Ti)] panthawi yotenthetsera. Aloyi ili ndi pafupifupi 24-27% nickel, 13.5-16% chromium, ndi zowonjezera za titaniyamu (1.9-2.35%), aluminiyamu (0.10-0.35%), molybdenum (1.0-1.5%), ndi vanadium (0.10-0.50%). Yapangidwira ntchito zomwe zimafuna mphamvu yayitali mpaka 700°C komanso kukana bwino okosijeni ndi dzimbiri.

Giredi 660 imadziwika ndi:

●Mphamvu yotentha kwambirimpaka 704°C (1300°F)

●Kukana bwino kwambiri kukwera ndi kuphulikakutentha kokwera

●Mvula yolimbakudzera mu chithandizo cha kutentha chokhazikika cha ukalamba

●Kukana kwabwino kwa okosijenimpaka 815°C

●Kukana kupumula kwa nkhawakutentha kwambiri

●Yopanda maginitokatundu

●Kupangidwa bwinondi kuthekera kwa makina

Kapangidwe ka Mankhwala

Chinthu UNS S66286 (ASTM) SUH660 (JIS) GH2132 (GB) Udindo
Nikeli (Ni) 24.0 – 27.0 24.0 – 27.0 24.0 – 27.0 Austenite stabilizer, kukana dzimbiri
Chromium (Cr) 13.5 – 16.0 13.5 – 16.0 13.5 – 16.0 Kukana kwa okosijeni, carbide wakale
Molybdenum (Mo) 1.0 – 1.5 1.0 – 1.5 1.0 – 1.5 Kulimbitsa njira yolimba
Titaniyamu (Ti) 1.90 – 2.35 1.90 – 2.35 1.90 – 2.35 mvula ya γ', kuuma kwa ukalamba
Aluminiyamu (Al) 0.10 – 0.35 ≤ 0.35 ≤ 0.35 mvula ya γ'
Vanadium (V) 0.10 – 0.50 0.10 – 0.50 0.10 – 0.50 Kukonza tirigu, carbide wakale
Boroni (B) 0.003 – 0.010 0.001 – 0.010 0.001 – 0.010 Kulimbitsa malire a tirigu
Cobalt (Co) ≤ 1.00 ≤ 1.00 ≤ 1.00 Chinthu chotsalira
Chitsulo (Fe) Kulinganiza Kulinganiza Kulinganiza Chigawo choyambira
Kaboni (C) ≤ 0.08 ≤ 0.08 ≤ 0.08 Carbide wakale
Silikoni (Si) ≤ 1.00 ≤ 1.00 ≤ 1.00 Chotsitsa mpweya
Manganese (Mn) ≤ 2.00 ≤ 2.00 ≤ 2.00 Chotsitsa mpweya
Phosphorus (P) ≤ 0.025 ≤ 0.040 ≤ 0.030 Kusayera
Sulfure (S) ≤ 0.025 ≤ 0.030 ≤ 0.020 Kusayera

Katundu wa Makina

Matenda a Annealed (Yankho Lochiritsidwa)

Katundu ASTM A453 Giredi 660 Mtengo
Kulimba kwamakokedwe ≤ 724 MPa (105 ksi)  
Mphamvu Yopereka (0.2% Kuchotsera) –  
Kutalikitsa ≥ 25%  
Kuuma ≤ 91 HRB

Ukalamba (Mvula Youma)

Katundu ASTM A453 Giredi 660 Zomwe Zachitika Kawirikawiri
Kulimba kwamakokedwe ≥ 965 MPa (140 ksi) 1,000 – 1,100 MPa
Mphamvu Yopereka (0.2% Kuchotsera) ≥ 655 MPa (95 ksi) 700 – 800 MPa
Kutalikitsa ≥ 15% 18 - 25%
Kuuma 24 - 35 HRC 28 - 32 HRC
Mphamvu Yoyenda (650°C, 100h) ≈ 240 MPa  
Mphamvu Yoyenda (700°C, 100h) ≈ 210 MPa

Katundu Wathupi

Katundu Mtengo
Kuchulukana 7.95 g/cm³
Malo Osungunula 1371 – 1427°C
Kutentha kwa Matenthedwe 15.0 W/m·K pa 150°C
Kuchuluka kwa Kutentha kwa Kutentha 16.8 × 10⁻⁶/°C (20-100°C)
Modulus Yotanuka 201 GPa
Kutha kwa Maginito Yopanda maginito

Ubwino Waukulu wa Inconel 660

Mphamvu Yotentha Kwambiri– Inconel 660 imasunga mphamvu yolimba, yotopa, komanso yophulika mpaka 704°C. Njira yolimbikitsira mvula ya γ' imapereka mphamvu yokwera kwambiri kutentha poyerekeza ndi zitsulo zosapanga dzimbiri za austenitic. Chitsulochi chimagwiritsidwa ntchito kwambiri pa mabotolo a turbine ndi zomangira komwe kukana kumasuka ndikofunikira.

Kukana Kwambiri kwa Kuphulika kwa Mphepete– Chitsulochi chimakhala ndi mphamvu yolimba kwambiri pa kutentha kwambiri. Moyo wake wozizira komanso kuphulika kwa chivundikirocho pa 650°C umaposa maola 1,000 pansi pa mphamvu yapakati, zomwe zimapangitsa kuti chikhale chodalirika pa ntchito zotentha kwambiri kwa nthawi yayitali.

Kusungunuka Kwabwino ndi Kukana Kudzimbiritsa– Ndi 13.5-16% ya chromium, Inconel 660 imapereka kukana bwino ku okosijeni, kukula, ndi dzimbiri lotentha kwambiri. Chitsulochi chimagwira ntchito bwino m'malo osungira okosijeni mpaka 815°C ndipo chimalimbana ndi zinthu zosiyanasiyana zowononga.

Mvula Yolimba– Inconel 660 imatha kuumitsidwa ndi kutentha kwa ukalamba. Nthawi yokhazikika yokalamba (675-705°C, maola 12-16) imapanga zinthu zabwino kwambiri zamakanika ndipo imapereka mphamvu yabwino kwambiri yopumulira kupsinjika, zomwe ndizofunikira kwambiri pakugwiritsa ntchito bolt.

Kukana Kutopa Kwabwino- Chopangirachi chimapereka kukana bwino kutopa ndi kutopa kwa kutentha, zomwe zimapangitsa kuti chikhale choyenera kugwiritsidwa ntchito pazinthu zomwe zimayendetsedwa ndi cyclic load pa kutentha kwakukulu. Izi ndizofunikira kwambiri pakugwiritsa ntchito turbine ndi zida za injini.

Kugwira Ntchito Bwino Kwambiri ndi Kutha Kugwira Ntchito– Inconel 660 ili ndi makina abwino kuposa ma superalloy ena ambiri. Itha kupangidwa mosavuta, kupangidwa motentha, komanso kupangidwa mozizira. Chitsulocho chimatha kuwotcherera pogwiritsa ntchito TIG, MIG, ndi welding yolimba pogwiritsa ntchito zitsulo zoyenera zodzaza.

Ubwino Waukulu wa Inconel 660

Mphamvu Yotentha Kwambiri– Inconel 660 imasunga mphamvu yolimba, yotopa, komanso yophulika mpaka 704°C. Njira yolimbikitsira mvula ya γ' imapereka mphamvu yokwera kwambiri kutentha poyerekeza ndi zitsulo zosapanga dzimbiri za austenitic. Chitsulochi chimagwiritsidwa ntchito kwambiri pa mabotolo a turbine ndi zomangira komwe kukana kumasuka ndikofunikira.

Kukana Kwambiri kwa Kuphulika kwa Mphepete– Chitsulochi chimakhala ndi mphamvu yolimba kwambiri pa kutentha kwambiri. Moyo wake wozizira komanso kuphulika kwa chivundikirocho pa 650°C umaposa maola 1,000 pansi pa mphamvu yapakati, zomwe zimapangitsa kuti chikhale chodalirika pa ntchito zotentha kwambiri kwa nthawi yayitali.

Kusungunuka Kwabwino ndi Kukana Kudzimbiritsa– Ndi 13.5-16% ya chromium, Inconel 660 imapereka kukana bwino ku okosijeni, kukula, ndi dzimbiri lotentha kwambiri. Chitsulochi chimagwira ntchito bwino m'malo osungira okosijeni mpaka 815°C ndipo chimalimbana ndi zinthu zosiyanasiyana zowononga.

Mvula Yolimba– Inconel 660 imatha kuumitsidwa ndi kutentha kwa ukalamba. Nthawi yokhazikika yokalamba (675-705°C, maola 12-16) imapanga zinthu zabwino kwambiri zamakanika ndipo imapereka mphamvu yabwino kwambiri yopumulira kupsinjika, zomwe ndizofunikira kwambiri pakugwiritsa ntchito bolt.

Kukana Kutopa Kwabwino- Chopangirachi chimapereka kukana bwino kutopa ndi kutopa kwa kutentha, zomwe zimapangitsa kuti chikhale choyenera kugwiritsidwa ntchito pazinthu zomwe zimayendetsedwa ndi cyclic load pa kutentha kwakukulu. Izi ndizofunikira kwambiri pakugwiritsa ntchito turbine ndi zida za injini.

Kugwira Ntchito Bwino Kwambiri ndi Kutha Kugwira Ntchito– Inconel 660 ili ndi makina abwino kuposa ma superalloy ena ambiri. Itha kupangidwa mosavuta, kupangidwa motentha, komanso kupangidwa mozizira. Chitsulocho chimatha kuwotcherera pogwiritsa ntchito TIG, MIG, ndi welding yolimba pogwiritsa ntchito zitsulo zoyenera zodzaza.

Kuchiza Kutentha kwa Inconel 660

Inconel 660 ndi aloyi yolimba yomwe imafuna kutentha kwapadera kuti ikwaniritse mawonekedwe abwino kwambiri a makina:

Kuthira Mayankho (Mkhalidwe A):

●Kutentha:980 – 1010°C (1800 – 1850°F)

●Nthawi Yothira:Ola limodzi

●Kuziziritsa:Kuziziritsa mwachangu (mafuta kapena madzi oziziritsira)

●Cholinga:Sungunulani ma precipitates onse, mukwaniritse gawo limodzi la austenite

●Zotsatira:Mkhalidwe wofewa, wogwira ntchito, wokonzeka kupangidwa ndi kupangidwa

Kuuma kwa Mvula (Kukalamba - Mkhalidwe B):

●Kutentha:675 – 705°C (1250 – 1300°F)

●Nthawi Yothira:Maola 12 - 16

●Kuziziritsa:Mpweya wozizira

●Cholinga:Fomu ya Ni₃(Al,Ti) γ' imathandizira kulimbitsa

●Zotsatira:Mphamvu yayikulu komanso kukana kukwawa

Kukalamba Kawiri (Njira ina):

● Gawo Loyamba: 705°C kwa maola 16, ng'anjo izizire mpaka 620°C

● Gawo Lachiwiri: 620°C kwa maola 16, mpweya uzizire

●Cholinga:Konzani kukana kupsinjika maganizo pa ntchito zomangira

Mafomu Opezeka a Zogulitsa kuchokera ku Womic Steel

Chitoliro Chopanda Msoko & Chitoliro Chopanda Msoko

●Chidutswa cha Kunja:6mm – 200mm

●Kukhuthala kwa Khoma:1mm - 25mm

●Utali:Mpaka 12m

●Miyezo:ASTM B639, ASTM B983, AMS 5731, AMS 5732, AMS 5737, AMS 5895

●Mapulogalamu:Mapaipi otentha kwambiri, machubu osinthira kutentha, mizere ya zida, machubu amlengalenga

●Mawu Ofunika:Chitoliro chopanda msoko cha Inconel 660, chubu cha Giredi 660, chitoliro cha UNS S66286, chubu cha SUH660, chitoliro chopanda msoko cha 1.4980

Chitsulo Chopingasa (Chozungulira, Chozungulira, Chosalala, Chozungulira)

●M'mimba mwake:6mm – 300mm

●Pamwamba:Yotenthedwa, Yowala (yozizira), Yophwanyika, Yozungulira

●Miyezo:ASTM A453, ASTM B639, AMS 5731, AMS 5732, AMS 5734, AMS 5737

●Mapulogalamu:Maboluti a Turbine, zomangira, ma stud, shafts, ma valve stems, ma machining stock

●Mawu Ofunika:Mpiringidzo wozungulira wa Inconel 660, Mpiringidzo wa Giredi 660, ndodo ya SUH660, ASTM A453 Giredi 660, zomangira kutentha kwambiri

Chitsulo ndi Mapepala

●Kukhuthala:1mm – 100mm

●M'lifupi:Mpaka 2000mm

●Miyezo:AMS 5525, AMS 5858

●Mapulogalamu:Zigawo za chotengera chopanikizika, ziwalo zomangira, malo opanda flange

●Mawu Ofunika:Mbale ya Inconel 660, pepala la Giredi 660, mbale ya alloy, mbale yotentha kwambiri

Chitsulo Chokulungira ndi Mzere wa Chitsulo

●Kukhuthala:0.5mm – 4.0mm

●M'lifupi:10mm – 1000mm

●Miyezo:AMS 5525

●Mapulogalamu:Zigawo zopangidwa, bellows, stampings

●Mawu Ofunika:Inconel 660 coil, strip, strip yotentha kwambiri

Ma Flanges ndi Zolumikizira

●Mitundu:Khosi Lolukidwa, Lotsetsereka, Losawoneka, Lolukidwa ndi Soketi, Lokhala ndi Ulusi

●Kukula:1/2" – 24"

●Kuyeza kwa Kupanikizika:Kalasi 150 - Kalasi 2500

●Miyezo:ASTM A453, ASME B16.5

●Mawu Ofunika:Ma flange a Inconel 660, zolumikizira za Giredi 660

Zopangira

●Mitundu:Mphete, ma disk, shafts, matupi a ma valve, ma geometries apadera

●Kulemera:Mpaka 3,000kg pa chidutswa chilichonse

●Miyezo:ASTM A453, AMS 5731

●Mawu Ofunika:Inconel 660 forging, forged ring, turbine component forging

Zomangira (Mabolt, Mtedza, Zidutswa)

●Mitundu:Maboluti a Hex, Zomangira za Socket head cap, Maboluti a Stud, Ndodo zolumikizidwa, Mtedza, Ma Washer

●Kukula:M2 – M100, 1/4” – 4”

●Miyezo:ASTM A453 Giredi 660, ASTM B637

●Mapulogalamu:Mabotolo a Turbine, maulumikizidwe a flange otentha kwambiri, zomangira zomangira

●Mawu Ofunika:Maboluti a Inconel 660, Maboluti a Giredi 660 stud, zomangira kutentha kwambiri, maboluti a turbine

Ma Valves a Giredi 660

●Mitundu:Ma valve a mpira, Ma valve a pachipata, Ma valve a Globe, Ma valve owunikira

●Kukula:1/2" – 12"

●Kuyeza kwa Kupanikizika:Kalasi 150 - Kalasi 2500

●Kuchuluka kwa Kutentha:-196°C mpaka +704°C

●Miyezo Yopangira Kapangidwe:API 608, API 6D, ASME B16.34

●Kuchitapo kanthu:Manja, Pneumatic, Magetsi

●Mapulogalamu:Kupatula kutentha kwambiri, mizere ya nthunzi ya turbine, kuwongolera turbine ya gasi

Giredi 660 vs. Inconel 718: Kuyerekeza

Inconel 660 ndi Inconel 718 zonse ndi ma superalloy ouma mpweya, koma ali ndi kusiyana kwakukulu:

Inconel 660 - Aloyi Yokhala ndi Chitsulo Chotentha Kwambiri

●Gawo Loyambira:Iron (yofanana) yokhala ndi 24-27% Ni

●Gawo lolimbitsa:γ' (Ni₃(Al,Ti))

●Mphamvu Yolimba (yokalamba):≥ 965 MPa

●Mphamvu ya kutentha:Kufikira 704°C

●Ntchito zazikulu:Maboluti a Turbine, zomangira, ma stud, zida za injini ya jet

●Mtengo:Yotsika mtengo kuposa 718 yochokera ku nickel

●Inconel 718 - Superalloy Yochokera ku Nikeli

●Gawo Loyambira:Nickel (50-55%) yokhala ndi 18-20% Fe

●Magawo olimbikitsa:γ' (Ni₃Al) + γ'' (Ni₃Nb)

●Mphamvu Yolimba (yokalamba):≥ 1,240 MPa

●Mphamvu ya kutentha:Kufikira 700°C

●Ntchito zazikulu:Ma turbine disks, ma rocket motors, mafuta ndi gasi a HPHT

Nthawi yosankha Giredi 660:Magwiritsidwe ntchito ofunikira maboliti ndi zomangira zotentha kwambiri, zida za injini ya jet, maboliti a turbine, ndi magalimoto ogwira ntchito bwino kwambiri komwe mtengo wake ndi chinthu chofunikira ndipo mphamvu yokwera mpaka 700°C imafunika.

Nthawi yosankha Inconel 718:Kugwiritsa ntchito komwe kumafuna mphamvu yayikulu kwambiri kutentha, kulimba kwa kusweka, komanso kukana kukwawa pa kutentha mpaka 700°C komwe mtengo wake suli wofunika kwambiri.

Miyezo ndi Mafotokozedwe

Muyezo Kufotokozera
Kusankhidwa kwa UNS S66286
Nambala ya Werkstoff 1.4980
AISI/SAE 660
ASTM A453 Mafotokozedwe wamba a bolting yotentha kwambiri
ASTM B639 Mzere/ndodo ya aloyi yotentha kwambiri
AMS 5525 Mbale/pepala/chidutswa
AMS 5731 Bala, waya, zomangira
AMS 5732 Bala, waya, zomangira
AMS 5734 Bala, waya, zomangira
AMS 5737 Chitoliro ndi chubu
AMS 5895 Bala, waya, zomangira
JIS SUH660
GB/T GH2132
Ku Ulaya 1.4980 / X6NiCrTiMoV25-15-2
ISO X6NiCrTiMoV25-15-2

Kugwiritsa ntchito Inconel 660

Zamlengalenga– Inconel 660 imagwiritsidwa ntchito kwambiri mu injini ya jet ndi zida za gasi kuphatikizapo ma turbine bolts, ma compressor disks, ma turbine casings, afterburner parts, ma thrust reversers, ndi zida zoyikira injini. Kuphatikiza kwake ndi mphamvu yotentha kwambiri, kukana kutopa, komanso kukana okosijeni kumapangitsa kuti ikhale yoyenera kugwiritsidwa ntchito kwambiri mumlengalenga. Alloy iyi ndi chinthu chokhazikika cha ma turbine ndi ma fasteners a injini ya jet omwe amagwira ntchito kutentha mpaka 700°C.

Kupanga Mphamvu ya Gasi Yopangira Turbine- Chitsulochi chimagwiritsidwa ntchito popanga maboluti a turbine, ma stud, ndi zomangira m'ma turbine a gasi a mafakitale, ma turbine a nthunzi, ndi malo opangira magetsi ophatikizana. Kukana kwake ku kupumula kwa kupsinjika pa kutentha kwakukulu kumatsimikizira kulumikizana kodalirika kwa maboluti kudzera mu nthawi yayitali yautumiki.

Magalimoto– Inconel 660 imagwiritsidwa ntchito m'nyumba zosungiramo zinthu zotayira mpweya, ma exhaust manifolds, zigawo za injini ya dizilo, ndi zomangira zamagalimoto zogwira ntchito kwambiri. Kutha kwake kupirira kutentha kwa mpweya wotayira mpweya komanso kutentha kwa mpweya kumapangitsa kuti ikhale yoyenera injini zamakono zogwira ntchito kwambiri komanso zotayira mpweya.

Mphamvu ya Nyukiliya- Chitsulochi chimagwiritsidwa ntchito mu zigawo za nyukiliya, mkati mwa core, makina owongolera ndodo, ndi zomangira kutentha kwambiri zomwe zimafuna kudalirika kwa nthawi yayitali komanso kukana kuwala kwa neutron.

Kukonza Mafuta– Inconel 660 imagwiritsidwa ntchito mu ma reactor a mankhwala otentha kwambiri, machubu okonzanso, zigawo za uvuni, ndi mapaipi opangira zinthu omwe amafunika mphamvu ndi kukana okosijeni pa kutentha kwakukulu.

Kuphimba Kotentha Kwambiri– Giredi 660 ndiye chinthu chokhazikika chogwiritsira ntchito ma bolting otentha kwambiri. Ma bolting ndi ma stud a ASTM A453 Giredi 660 amasankhidwa kwambiri kuti agwiritsidwe ntchito pa ma flange a zotengera zopanikizika, ma turbine casings, ndi ma payipi olumikizira kutentha kwambiri omwe amafunika kukana kugwedezeka ndi kupumula.

Mafunso Ofunsidwa Kawirikawiri

Q: Kodi Inconel 660 ndi chiyani?

A: Inconel 660 (UNS S66286 / SUH660 / GH2132) ndi chipangizo cholimba cha precipitation-harding chomwe chimagwiritsa ntchito chitsulo chokhala ndi mphamvu yabwino kwambiri yotentha mpaka 704°C. Chimalimbikitsidwa ndi precipitation ya γ' kudzera mu kutentha kokalamba ndipo chimagwiritsidwa ntchito kwambiri pa ma turbine bolts, zomangira, ndi zigawo za injini ya jet.

Q: Kodi kusiyana pakati pa Giredi 660 ndi Inconel 718 ndi kotani?

A: Inconel 660 imagwiritsa ntchito chitsulo (yokhala ndi 24-27% Ni, balance Fe) yokhala ndi mphamvu yokoka ≥ 965 MPa, pomwe Inconel 718 imagwiritsa ntchito nickel (50-55% Ni) yokhala ndi mphamvu yokoka ≥ 1,240 MPa. Giredi 660 ndi yotsika mtengo komanso imagwiritsidwa ntchito kwambiri popangira bolting; Inconel 718 imagwiritsidwa ntchito popangira mphamvu kwambiri.

Q: Kodi kutentha kwakukulu kwa ntchito ya Inconel 660 ndi kotani?

A: Inconel 660 yasankhidwa kuti igwire ntchito mosalekeza mpaka 704°C (1300°F). Pakukana okosijeni, kuyenda kwakanthawi kochepa mpaka 815°C (1500°F) n'kotheka. Mphamvu yokwera imachepa kwambiri kuposa 700°C.

Q: Kodi Inconel 660 ndi yosavuta kuiwotcherera?

A: Inde, Inconel 660 ikhoza kulumikizidwa pogwiritsa ntchito njira za TIG, MIG, ndi resistance welding. Komabe, kuwotcherera kumafuna kuwongolera mosamala kutentha komwe kumalowetsa komanso kusankha zitsulo zodzaza kuti zisasweke. Kuphimba ndi kukalamba kwa yankho pambuyo pa weld kungafunike kuti mubwezeretse mawonekedwe a makina.

Q: Kodi mawu ofanana ndi Inconel 660 ku China ndi ati?

A: Chofanana ndi Inconel 660 cha ku China ndi GH2132 (高温合金) pa ntchito zapamlengalenga ndi kutentha kwambiri, ndipo chofanana ndi cha ku Japan ndi SUH660.

Q: Ndi mitundu iti ya zinthu zomwe zilipo za Inconel 660?

A: Womic Steel imapereka Inconel 660 mu chitoliro chopanda msoko, chitoliro cholumikizidwa, bala lachitsulo, mbale yachitsulo, cholumikizira chachitsulo, mzere, ma flange, zolumikizira, zolumikizira, waya, zomangira, ndi ma valve. Mafotokozedwe athunthu azinthu ndi kukula kwake zalembedwa mu gawo la kupezeka kwazinthu.

Q: Kodi Inconel 660 imafuna chithandizo cha kutentha?

A: Inde. Inconel 660 imafuna kupopera madzi (980-1010°C) kutsatiridwa ndi kukalamba (675-705°C kwa maola 12-16) kuti ikwaniritse bwino ntchito zamakina. Chithandizo cha ukalamba chimalimbikitsa gawo la γ kuti likhale lolimba.

Lumikizanani ndi Womic Steel

Webusaiti: www.womicsteel.com
Imelo: sales@womicsteel.com

Foni / WhatsApp / WeChat:

Victor: +86 15575100681

Jack: +86 18390957568

Chitsulo cha Womic – Mnzanu wodalirika wa Inconel 660 / Giredi 660 (UNS S66286, SUH660, GH2132) chitoliro chopanda msoko, bala lachitsulo, mbale yachitsulo, coil yachitsulo, ma flanges, zolumikizira, zomangira, ndi zomangira zomangira ndege, turbine ya gasi, kupanga magetsi, ndi ma bolting otentha kwambiri padziko lonse lapansi. Kutsata kwathunthu, satifiketi ya gulu logawa, ndi zikalata za EN 10204 Type 3.1/3.2 zilipo.